The high intensity of the main peaks in XGO confirms the presence of a large amount of oxygen functional groups after the oxidation process.
After the XGO was reduced, hydroxyl and alkoxy groups were significantly decreased (Figure 3(c)), and the phenol C=C ring stretching at 1585 cm−1 was present [10].