Here, the experimenter prints a large design (on the order ofseveral millimeters) onto the Shrinky Dink film using a
conventional laser printer, and, upon heat treatment, the shrink film polymer contracts, reducing the size of the printed design to a scale of several hundred micrometers. We extended this approach to the high school laboratory because