It was shown that the highest possible filler level was all the more high when decreasing fibre size, due to reduced film heterogeneity and improved wetting of fibres by the polymer
It was shown that the highest possible filler level was all the more high when decreasing fibre size, due to reduced film heterogeneityand improved wetting of fibres by the polymer