Using the proposed setup, a successful machining of ZrO2 ceramics is performed, even after the starting layer is completely removed (Fig. 14).
Bores with an aspect ratio 5 could be manufactured using Y2O3- (Fig. 15) as well as MgO stabilized ZrO2 material