it was smoother after the reaction in the FBR had proceeded for
3 months. Moreover, Fig. 3b and d shows details of the original
activated alumina grain support with a typical sheet-like structure
and the surface of the FeAA with fine granular structure.
The specific surface areas of the original activated alumina grain
support and FeAA are 127 and 170 m2 g−1, respectively