The MARM parameter space included a laser power and scan speed range of 300-600W
and 100-300 mm/s respectively and the CMSX parameter space included a scan speed range of
400-900 mm/s while the laser power was held constant at 500 W. In the case of the MARM
experiments, two samples were produced for every parameter combination. One sample was
analyzed in the as-processed condition and the second went through a post-process stress relief
heat treatment in an argon purged tube furnace for 4 hours at 1060 °C.