Moderate amounts of filler and amino silane were added
to acetone. After more than three hours of agitation at
ambient temperature, the filler, whose surface was coated
with silane, was obtained using a filter. The obtained filler
was then placed in a vacuum oven at 120oC for two hours
to dry