able 1
Solution properties of the electrospraying solutions with the following compositions:
WPC (20% w/v of WPC in water + 5 wt.% Span 20); resistant starch (20% w/v resistant
starch in water + 0.5 wt.% guar gum + 5 wt.% Span 20). The solutions with folic acid
additionally contained 1.5 wt.% of the bioactive with respect to the biopolymer
weight.