Aramid fabric used in this study is the plain weaved structure
Kevlar 129. Three types of kenaf fibres were used in this study:
woven, unidirectional and mat. The woven kenaf was produced
by the interlacement of warp and weft yarns by using table
loom. The yarns were obtained from local suppliers, Innovative
Pultrusion Sdn Bhd. The unidirectional samples consist of
kenaf yarn (800 tex) cross plied at 0°/90°. No chemical treatment
was conducted on the kenaf fibres prior to this study.