Quantity of CDS added during the production
process had an inverse relationship with the onset and
midpoint transition temperature of DDGS. The low glass transition
temperature of plasticizer components in DDGS, glycerol, and low
molecular weight sugars might have also influenced the glass
transition behavior of DDGS.