From each of the six shortest bundle sections, one set, and from each of the remaining 12 bundle sections, two sets of three tensile test specimens with nominal gauge lengths lg = 50 mm, 125 mm and 250 mm were cut, yielding a total of n = 30 specimens per gauge length. All specimens were sintered for 1 h at a temperature of 1300◦C in air.