To investigate the water absorption capability of the recycled cellulose aerogel,
the aerogel samples were subjected to three cycles of water absorption tests using a dip coater for 2 h (Fig. 3).
The size and weight of the sample were measured before and after each test.
The wet sample was then dried at room temperature for seven days.