The XRD result of the recycled catalysts (as presented in Fig. 2b) shows the partial transformation of CaO phase (2h = 37.6 and 54.2) to Ca (OH)2 phase (2h = 34.2) upon the repeated use of catalyst, which is
probably due to CaO reacts with water presents in the reactants and/or moisture upon the repeated use of catalyst.