At a given loading and without Si-69, the PSi-filled
composite shows lower rolling resistance than the
corresponding FSi-filled composite because PSi has lower
surface area and volume fraction. Nevertheless, the rolling
resistance of both silica-filled composite systems reduces
and is comparable when Si-69 is incorporated.