water-to-cement ratios were investigated. Table 2 shows the concrete mix details. The concrete was mixed first, then cast, and demoulded, Afterwards it was cured for 28 days in a controlled environment before the accelerated carbonation test.
water-to-cement ratios were investigated. Table 2 shows the concretemix details. The concrete was mixed first, then cast, anddemoulded, Afterwards it was cured for 28 days in a controlledenvironment before the accelerated carbonation test.