The ratio of the WPC scrap:WPC freshfeed at 30:70 was found to be the most appropriate
The number of re-processing passes by 35% and 30% respectively, was detected in the both M n and the M w was decreased
tensile and flexural strength, while higher flexural modulus. The lower strength of the recycled samples was in good agreement with their lower density.