The photographs of decal substrates
after hot-pressing are presented in Fig. 2. Both anode and
cathode catalyst layers are successfully transferred under all
the applied pressures, with the exception of 0.5 MPa (Fig. 2(a)),
where transfer is incomplete. In some cases, only traces of
catalyst are left on the substrate films particularly near the
edge region of the electrodes.