At the
first 20 days hydrolysis, the mass loss almost does not happen. In
the next 15 days, the mass decreases rapidly and lost about 20% at
35 days hydrolysis. Similarly, no visible difference of mass loss can
be found between neat PLA and PLA/NR blends even though the
moisture absorption are different from each other.