The results show that the pretreatments (acid and alkaline) were
efficient in reducing the hemicellulose (from 29.6 to 12.2%) and
lignin (from 19.4 to 9.3%) fractions, with a concomitant increase in
the cellulose content of cellulignin from 34.1% to 68.0%.