In order to improve the catalysts basicity a commercial CaO material was impregnated with aqueous solution of lithium nitrate (Li/Ca = 0.3 atomic ratio). The catalysts were calcined at 575 ◦C and 800 ◦C, for 5 h, to remove nitrate ions before reaction