Sample was allowed to rest for at least 5 min to attain thermal equilibrium and relaxation. Then, a frequency (v) sweep test was performed from 100 to 0.1 rad/s at 0.05% strain. Data obtained were elastic modulus (G0), viscous modulus (G00), and loss tangent (tan d = G00/G0).