Therefore multiple washing cycles used in conjunction with bath ultrasonication in fresh ethanol are needed for the removal of residual potassium [23]. After this the GO was dried and pulverized again. Finally, the GO was heated to 1050 8C and held in the furnace for 30 s to form graphene.