Powder X-ray diffraction (PXRD) analysis was repeated over a month
to confirm the irreversibility of the transition. Whereas small
crystalline impurities (e.g., untransformed starting materials) are
common in the aT-ZIFs, no such impurities were observed in the
am-ZIFs.