We examined redispersion processing time that is required for making the difference reflecting the aggregation forces between colloidal particles. Redispersed layer of the model dispersions with no salt or 100 mM NaCl underwent turbidimetric measurements 0, 20, 40 and 60 min after the redispersion treatment by the contact speaker