At first, all components were measured separately using TGA
either in nitrogen or in oxygen atmosphere. Afterwards, method
development was accomplished with WPC test pieces of known
composition (Table 1). Initially, all components were measured
un-dried. However, it could be observed that the content of moisture in wood floor and WPC scattered strongly (Figs. 3 and 5).