The calcination temperature strongly affected the degree of crystallinity of MWT walls. The amount of WO3 in the host TiO2 matrix also played an important role on the crystallinity: the WO3 crystal phase was not able to be detected in M1W8T samples calcinated at both 500 and 600 C due to the small amount.