In these experiments, 1.6-2.6 kg of the feedstock was fed into the pyrolysis reactor. The pyrolyzer and the
reformer were then heated up to the preset temperatures. The catalyst (100 g) was loaded in the catalytic reforming
reactor, where the pyrolysis gas generated in the first reactor was reformed. After having the reforming reaction, the