In the co-precipitation synthesis, Sr(NO3)2 and Mg(NO3)2 aqueous solutions were mixed together and 0.1 M (NH4)2CO3 solution was then added drop wise to precipitate the product.
The precipitate was collected and then calcined at desired temperature.
This sample is denoted Sr/MgO-C.