were incorporated
in cells comprising one positive and two negative plates.
Commercial plates with lead–calcium grids and 10 Ahcapacitywere
used. H2SO4 solution of 1.28 g cm−3 densitywas used as electrolyte
at 96% saturation and 20% compression of the active block. A total
of six test cells were assembled as follows: