Set up 3 electrode system using GC electrode as the working electrode, Pt rod as the counter electrode, Ag/AgCl as the reference electrode, and 10 mL 0.5 M H2SO4 as electrolyte solution. Degas the solution by purging with N2 or Argon for about 5 min.