Eachcylindrical sample piece was compressed on the uniaxial compressing stage (50 mm/min) of a Rheometer" (FUDO Kogyo K.K., Tokyo, Japan) with a spherical plunger ( =5 mm) and the force versus deformation curve was recorded on a chart with a full scale of 200 g at chart speed of 100 mm/min.