Table 2 shows the percentage of volatile solid (VS) in total solid
(TS) of the untreated and treated pine woods. The VS of untreated
sample was 86% which was increased by the pretreatment. The results
of Table 2 also show that prolongation of the pretreatment increased
the VS content, indicating the higher biodegradable
material content in the treated materials.