may have also contributed to
strength losses. However, this was beyond the scope of this
work and there was insufficient data to quantify the effect of
these parameters individually.
In contrast to normal weight concrete, where curing at
elevated temperatures can accelerate the pozzolanic reaction
[45] and enhance concrete strength development [43,46], the
majority of the PC/FAf HBC foamed concretes with 600 kg/