The chemical composition before and after the pretreatment
of the raw materials is presented in Table 2. The estimated crystallinity
index using XRD and Raman is shown before and after
the mechanical treatment in the table. The chemical composition
showed a considerable amount of cellulose for carrot residue prior
to the chemical treatment, with 45% compared to 17% for BSG