specialized PC films, 0.125 mm and 0.2 mm thick, respectively, were custom manufactured for the IMD process used in this experiment. the film was baked in the oven for 40 min at a temperature of 80C to de-moisturize it. then a grid was printed on the surface of the film using printing ink of series before forming as depicted in fig1.