As for pure PVA, the former sharp tanı peak (around80 ◦C) is obviously related with Tg, which is assigned to ˛a relaxation in the amorphous region of PVA; the other one is located at about 135 ◦C. which is attributed to ˇc dispersion because of PVA
crystalline relaxation