limited by thermodynamics to the amount of carbon monoxide that
can be shifted. Therefore, a lower temperature reactor (210–330 8C)
is used to convert the carbon monoxide to a lower level. High
temperature WGS reactors commonly use an iron catalyst, and
lower temperature reactors often use a copper catalyst [10–14].