Modulus at 100 percent, pulling the stretch of the composite rubber with an increase in value. As the uv radiation duration increases and the tensile strength increases to 45 minutes, the UV coverage period is reduced and decreases when more UV rays are projected. Meanwhile, the pre-elongation value is reduced.