It should be noted that the LbL film-coated silk has a higher
weight percentage than the pristine one at the temperature above
330 C. Moreover, curves of the functionalized silk fibers reach
equilibrium at around 740 C, which is 90 C higher than the equilibrium
temperature of the pristine one.