From the mid-1980s and continuing until the present time, a typical EAF wear lining for the production of carbon and low-alloy steels consists of water-cooled panels in the upper and middle sidewalls from just above the slag lines and several resinbonded magnesia-graphite qualities in the slaglines and lower hot-spot sidewalls.