About these casting test , have we hole or solid in center location
Please see reports as following
1. 400P12I (CD) Porosity (Version5) → hole in center location
2. 400P12I Porosity (Version6) →40 % Solid in center location
We need to check any parameter for find and improve porosity problem
Mr. Supachai
Can you confirm dada as following