Friction materials having balanced energy
absorption coefficient and other friction properties has been
prepared by compaction and press sintering (750-850 oC, 1-
10 MPa) of a mixture containing Sn (2-8 wt.%), SiO2 (2-10
wt.%), rice husk (2-8 wt.%) and rest electrolytic Cu powder