Humidity of the samples increased with cellulose addition, taking longer time as shown in Fig. 3. Starch–gelatin polymer
matrix reached an equilibrium at 33 min, while the starch–gelatin with cellulose took up to 50 min, meaning that this
moisture is bound water in the material