The microhardness of the anodic films progressively decreased with increasing electrolyte temperatures whereas the wear resistance remained constant for the lower considered temperatures from 5 °C to 25 °C ,followed by a decreasing wear resistance with increasing
electrolyte temperature from 25 °C onwards.