For the two-step sintering process, the sintering procedure was programmed from room temperature to the firststep sintering temperature T1°C with a rapid heating rate 10° C/min without any socking time, and then rapidly cooled to a lower second-step temperature T2°C at 30°C/min, then held for a long time t h