Addition of Joncryl
significantly improved film tensile strength, 0.2% offset
yield strength, and elongation, especially evident with the
250% elongation of 70/30 (TPS/p-PLA) film. Total surface
energy of films was not significantly influenced by addition
of Joncryl.