The
finding indicates that the crystallinity of the
obtained anatase particles increased as the pH
values of the aqueous solutions were between 2.0
and 3.0. In general, the full width at halfmaximum
of XRD peak corresponds to the crystal
size of porous materials. When the width was
broader, the crystallites exhibited smaller size.