0.75BF–0.25BT ceramics doped with 0–0.7 wt% MnO2 were prepared by a
conventional ceramic process. The samples were sintered at 940–
1020 °C in air, and their densification, phase evolution, microstructure
development, and piezoelectric properties were
examined.