The powder samples were pelletized and sintered at 500 °C for 6 h using Apex hydraulic press and a muffle furnace for temperature dependent electrical resistivity measurements by four point probe measurement setup.
The powder samples were pelletized and sintered at 500 °Cfor 6 h using Apex hydraulic press and a muffle furnace for temperature dependent electrical resistivity measurements by fourpoint probe measurement setup.