25 mL of polyol and equal proportion of isocyanate solution were mixed together using a flat stirrer to form a homogenous mixture.The mixture was kept undisturbed for a few minutes to achieve complete foaming. After completion of foaming, it was placed in an open at mosphere for 20 min to get a rigid structure and cut in to small cubes of desired size for the further studies.